汽轮机铜沉积技术分析及解决方案 王 柱1 ,宫有成2 ,张振华3 ,王礼君1 (1. 黑龙江省电力科学研究院,黑龙江哈尔滨150030; 2. 山东百年电力发展股份有限公司,山东龙口265700; 3. 华能山东辛店电厂,山东淄博255000) 摘 要: 分析了汽轮机高压缸铜化合物沉积的原因。针对铜沉积过程提出了去除铜沉积物的方法和防范铜沉积的措施。 关键词: 汽轮机;铜沉积;凝汽器;溶氧;化学清洗 中图分类号: TM621. 8 文献标识码: B 文章编号: 1002 - 1663 (2005) 01 - 0055 - 03 Technology analysis and its countermeasure of copper deposition on turbine WANG Zhu1 , GONG Youcheng2 , ZHANG Zhenhua3 , WANG L ijun1 (1. Heilongjiang Electric Power Research Institute, Harbin 150030, China; 2. Shandong Century PowerDevelopment Company, Longkou 265700, China; 3. Shandong Xindian Electric Power Plant of Huaneng Group, Zibo 255000, China) Abstract: The reasons caused copper and its compound deposited on the high p ressure cylinder of turbine were analyzed in the paper. The methods of copper deposition removal and the measures p reventing copper from deposition on the high p ressure cylinder focusing on the depositing character of copper were p resented in the paper. KeyWords: turbine; copper deposition; condenser; dissolved oxygen; chemical cleaning 一些凝汽器、给水加热器的管材为铜合金的大容量机组,当铜及其氧化物在汽轮机高压缸叶片上沉积时发电能力会降低。国外1台额定负荷为525MW亚临界机组,由于铜氧化物沉积在汽轮机高压缸末端使蒸汽通流部分发生阻塞而导致机组出力损失近10%。本文以这台机组为例,研究铜沉积的过程和机理,以便提出解决措施。 1 汽轮机铜沉积的危害 该亚临界机组凝汽器管材为铜97. 5%和钢2. 5% ,低压加热器的材质为海军黄铜, 4台高压加热器最初使用70 /30的铜/镍合金管,后将2台高加更换为不锈钢管。如图1所示, 1984~1986年,因铜的大量沉积而造成机组发电能力严重下降,须每隔2~3年进行喷砂处理。 图1 铜沉积造成的机组发电能力下降 2 汽轮机铜沉积产生过程和原因分析